Already Registered? Please sign in.


September 28, 2009

In this post, John Britt explains that giving a bit more consideration to kiln wash might help potters avoid some of the common kiln wash headaches - like scraping cracked kiln wash off shelves or lamenting an otherwise perfect piece that was ruined by a flake of kiln wash. Plus he shares some kiln wash recipes for various firing techniques.

September 23, 2009

Today, salt and wood firing potter Michael Kline takes us through his wadding process sharing his wadding recipe and tips for successful stacking in the kiln. He also explains how he adds sea shells into the mix for a nice flashing effect.

September 14, 2009

Today's post is an excerpt from our new free download, Wood Kiln Firing Techniques and Tips, in which Nesrin During shows us how to combine wood firing and raku firing. As you'll see, wood firing isn't just about high firing. You can build a simple raku kiln and fire your work with wood to get stunning results.

July 18, 2008

This week’s Video Tip of the Week is a follow-up video on trimming and glazing the wire-faceted bowls Mark Peters demonstrated last week. In today’s video, Mark shares a Cone 10 Temmoku glaze recipe and Randy Johnston’s flashing slip recipe, which he likes to use on these forms. We have also posted these recipes on the site so you don’t have to worry about jotting them down while watching the video. Enjoy! -Jennifer Harnetty, editor.