Tagged:  Joan Carcia

Announcing Winners of 2011 Potters Council Juried Show

Posted On October 14, 2010 1 Comment
  Potters Council is thrilled to announce the members chosen to participate in the 2011 Juried Exhibition, “The Shoulders We Stand On”. The show is being held in conjunction with the National Council on Education for the Ceramic Arts (NCECA) conference. “The Shoulders We Stand On” The 2011 Potters Council members show in Tampa, Florida… Read More »

Joan Carcia’s Terra Sigillata Recipe

Posted On March 26, 2008 1 Comment

On Monday, we brought you Joan Carcia’s saggar-firing technique. Today, as promised, we’ll share the other secret to her success with this technique: her terra sigillata recipe. Enjoy!


Building, Packing and Firing Saggars

Posted On March 24, 2008 4 Comments

This week, we will take a look at how Carcia uses terra sigillata, vegetation, oxides and salts to make her vividly colored work.