January 23, 2009
Ceramics Decorating Video: Inlaying Colored Clay Decoration into Handbuilt Vessels
Way, way back, while I was on maternity leave (such a distant memory now - sigh), Sherman Hall ran a video clip from Mitch Lyon's full length DVD, Handbuilding with Mitch Lyons, in which Lyon's demonstrated the broomstick method of handbuilding pottery. The technique intrigued me and I finally had a chance to check out the rest of the video. And it's a good one. So today thought I would send out a "part deux." In this clip, Lyons demonstrates how he inlays figurative colored clay motifs into his broomstick vases. I have included a step-by-step recap of the technique below, in addition to pointing you toward another great project for colored clay inlay from the Ceramic Arts Daily Feature ...