An Introduction to Salt-Soda Firing – Kiln Considerations and Loading Techniques that Enhance Results
In today’s video, Gordon Hutchens gives us a quick introduction to the salt/soda firing technique. He explains some of the considerations that go into building a salt/soda kiln (do not try this in an electric kiln or any other kiln that you wish to use for any other type of firing!). He also discusses some of the ways you can get great decorative results from the way the ware is placed in the kiln. If you wanted to know more about salt/soda firing, this video is a great place to start!