August 10, 2009
Rustic Handbuilt Work Blurs the Lines Between Functional Pottery and Ceramic Sculpture
Today, Joseph Pintz shares his clay body and glaze recipe he uses to give his work that vintage, rustic look. Plus he talks about the process behind his rough-hewn, handbuilt pottery.