December 3, 2008
Inspired by Terra Sigillata: A New Twist on an Ancient Surface Technique
When I think of terra sigillata, I think of the soft, satin surfaces of low-fired earthenware, like Greek red and black ware that still has that great surface sheen. But Anne Fløche has taken terra sigillata in a different direction. She's allowed herself to use it in a way that goes against tradition, but is true to her own inspiration and way of working. This is a classic example of taking a tried-and-true technique and making it personal. Whether you're using terra sigillata in a traditional manner or pushing it to try something new, Fløche provides a great tutorial (and a recipe) for making this versatile material.