In ceramics, finding the perfect glaze for your work is only part of the challenge. If the application is sloppy, it will show in the finished glazed piece!

 

So in today’s post, Frank James Fisher shares some handy tips to make sure your glaze goes on right. He also shares recipes for three cone 6 glazes that work very well together. –  Jennifer Harnetty, editor.


 

Always wipe bisqueware before firing to ensure a clean surface for the glaze to cling to, otherwise glaze can slide off  an unwiped pot onto a kiln shlef during firing.

Always wipe bisqueware before firing to ensure a clean surface for the glaze to cling to, otherwise glaze can slide off an unwiped pot onto a kiln shlef during firing.

Glazing Tips

 

Glaze needs a firm clean surface to cling to, so always wipe bisqueware before glazing to prevent glaze from sliding off onto a kiln shelf during firing.

 

Glazing very dry bisque surfaces can result in an extra-thick glaze application, because the moisture from the wet glaze is quickly absorbed into the dry bisque, causing a thick layer of glaze to adhere. Wiping the surface with a damp sponge before glazing yields a thinner glaze layer. Don’t use too much water, however, which may cause the glaze to run off the bisque resulting in a thin or uneven coat.

 



This post is an excerpt from Glazing Techniques!
Learn more and download an excerpt here!

 


 

recipe2The best sponges for glazing are the large wallpaper sponges sold at building supply stores. These sponges have small pores and are excellent for wiping wet glaze off pots. A large-pore sponge doesn’t last as long and leaves uneven edges.

 

If you need to wipe glaze off your pot, do so while the glaze is still wet. Wet glaze is removed more easily and results in less staining than if you wait until the glaze is dry on the pot.

 
recipe3recipe1

 
 

 


Article printed from Ceramic Arts Daily: http://ceramicartsdaily.org

URL to article: http://ceramicartsdaily.org/pottery-making-techniques/ceramic-glazing-techniques/glaze-recipes-and-expert-tips-for-great-pottery-glazing-results/

Copyright © 2008-2012 Ceramic Arts Daily. All rights reserved.