- Ceramic Arts Daily - http://ceramicartsdaily.org -
Less is More: A Minimalist Approach to Glazing Ceramics
Posted By Karen Swyler On February 17, 2010 @ 8:58 am In Ceramic Decorating Techniques,Daily,Features | 24 Comments
|
Today, in an excerpt from an upcoming Ceramics Monthly profile, Karen explains a little about how she approaches her glazing. I love her minimalist aesthetic and I plan to do some experimenting with the less-is-more approach to glazing. Should be fun! – Jennifer Harnetty, editor.
|
|
|
My glazing decisions are strongly influenced by my forms. Linear patterns and soft colors are employed to emphasize shape and add further layers of detail. Although large areas of the surfaces of these works are frequently unglazed, I spend a great deal of time preparing for the glazing process.
Prior to glazing, I sand my bisqueware with wet-dry sandpaper. This makes the unglazed surfaces smooth; the surface is almost marble-like once it has been fired.
|
|
|
For more great ideas for decorating pottery, be sure to download your copy of Getting the Most out of Ceramic Glazes and Underglazes: Using Commercial Ceramic Glazes and Underglazes to Achieve Color, Depth, and Complexity, which is free to Ceramic Arts Daily Subscribers. |
|
|
After sanding, I use automotive detail tape to create lines that will be glazed. This tape works particularly well to make a smooth, yet curved line on a variety of forms because it is slightly stretchy. The narrowness of the tape also allows me to make a series of thin lines close together. It adheres well to the bisque ware, but it is important the pieces are allowed to dry after sanding, because it will not stick if the bisqueware is damp.
|
|
|
Once the taping is complete, glaze is applied using a spray gun. Immediately upon completion of glaze application, the tape is removed and the glazed line remains. Additional detail cleanup is done with a sponge and a small knife.
To learn more about Karen Swyler and see more images of her work, please visit http://karenswyler.com. |
Article printed from Ceramic Arts Daily: http://ceramicartsdaily.org
URL to article: http://ceramicartsdaily.org/pottery-making-techniques/ceramic-decorating-techniques/less-is-more-a-minimalist-approach-to-glazing-ceramics/
Click here to print.