ZnO—High-temperature flux that promotes brilliant glossy surfaces. In some glazes can encourage opacity. With titanium in low-alumina glaze can encourage macrocrystalline growth (crystalline glazes). Volatizes in high-fire reduction. Toxic in inhalation.