Soluble metallic salt. Fuming agent to create mother-of-pearl luster on glazed surfaces. Introduced in cooling ramp at dull red heat, which will affect everything in kiln. Highly toxic in inhalation and ingestion. Fumes are especially toxic. Source: Clay: A Studio Handbook