Na2O×Al2O3×6SiO2—feldspars contributing sodium (and potassium), primarily as a high-temperature flux. Kona F-4 feldspar, NC-4 feldspar and nepheline syenite. Toxic in inhalation. Source: Clay: A Studio Handbook