Na2CO3—soluble source of soda, used as deflocculant, or to supply soda in vapor-glazing process. Source of flux in Egyptian paste recipes. Brush solution over hi-fire glaze to increase carbon trapping. Highly toxic in inhalation and ingestion. Skin irritant. Source: Clay: A Studio Handbook