rutile

Titanium ore, used as source of titanium dioxide, contains iron, other trace minerals—gives tan color, promotes crystallization giving mottled multicolor effects in some HT glazes, or in overglaze stain (very refractory, use sparingly). Gives rich mottled medium blue in some HT glazes. Dark rutile contains higher percentage of iron.