Al2O3×4SiO2×H2O—used in HT claybodies (20% or less) to reduce thermal expansion, increase thermal shock resistance, reduce shrinkage, give stronger vitreous bodies. May reduce plasticity. Source: Clay: A Studio Handbook
Al2O3×4SiO2×H2O—used in HT claybodies (20% or less) to reduce thermal expansion, increase thermal shock resistance, reduce shrinkage, give stronger vitreous bodies. May reduce plasticity. Source: Clay: A Studio Handbook