outgassing
The escape of gases from clay and glazes during firing. Carbonates, sulfates, nitrates, organic contaminants, and chemically combined water volatize between 600 and 1200° F. Other compounds, especially fluxes, volatize later during glaze-melt. See carbon coring, oxidation cleanup, water-smoking stage.