noborigama

Translates as “step-climbing kiln”—traditional Japanese multichamber downdraft/crossdraft climbing kiln, with initial firebox at bottom, and secondary fireboxes in each chamber. As kiln is fired, each chamber preheats the next. See climbing kiln.