lead silicate

3PbO×2SiO2—fritted lead compounds—LT flux, but resulting glazes may be toxic and should not be used on functional wares. Most powerful of all fluxes, promotes smooth-flowing, self-healing glazes. Highly toxic in inhalation and ingestion.