CMC Gum, Veegum Cer—water soluble organic thickeners often added to glazes or slips as a suspension and/or brushing agent. Also used to allow glaze adhesion to vitrified or previously glaze-fired surfaces. Most commercial low-fire glazes and underglazes contain gum additives. Source: Clay: A Studio Handbook