glaze, glazes, reduction-fired glazes, celadon, temmoku, chun, crystalline glazes, macrocrystalline glazes
Coating of powdered ceramic materials, usually prepared and applied in water suspension, which melts smooth and bonds to clay surface in glaze firing. See interface.