Gerstley borate; colemanite; calcium borate
CaO×3B2O3—traditional important LT alkaline flux, but is no longer being mined. Replace with Ferro 3134 for LT glazes, commercial Gerstley borate substitutes for HT glazes. Test all substitutes.