MgSO4—water soluble, rarely used as magnesium source in glazes. Most often used as flocculant for slips and glazes. Often added to porcelain and porcelaineous stoneware bodies (1/2 of 1% of dry materials weight) to counteract deflocculating alkalinity released by kaolins or fluxes.