Carboxymethylcellulose (CMC) — an organic gum used as a suspension/adhesion agent in glazes. Normally, a small amount of gum is added to a quart or so of warm water and left overnight. Once dissolved, this solution may be added in small doses to glazes, slips, and engobes to improve application performance. Source: Clay: A Studio Handbook