ball clay

Al2O3×2SiO2×2H2O —Secondary clays deposited in marshy areas. Very fine particle size, high plasticity, high in organic contaminates, and fires white or off-white. Used as the primary plasticizing clay in most claybodies, but in large quantities promotes high shrinkage.