anagama
Translates “cellar kiln”—Traditional Japanese kiln evolving from the bank-kiln, and featuring a long, swelling inclined tubular ware chamber, with lower extreme serving as firebox. Characteristically produces heavy flame-flashing and residual-ash effects.