This is a technique brought to us by Mark S. Richardson. The basic process has been around for quite a while, and has been known by different names, one of which is “naked raku” (but don’t go getting your hopes up-it’s not that kind of story). As with any firing process, you should wear protective clothing, and exercise all fire-safety precautions. Richardson devised a system for getting peel-away slip onto his pots, keeping the slip intact through the firing and reduction process, and then removing it easily at the end. - Sherman Hall, co-host, Ceramic Arts Daily.
|
Tags: Ceramic Decorating Techniques, naked raku
c | December 15th, 2009 at 7:52 pm
I have done naked raku with varied results. I have also experimented with a variety of slips. This fiberglass has made a world of difference in my results. I now do not have to redo as many when they shed their clothing too soon. Thanks for the tip.