- Ceramic Arts Daily - http://ceramicartsdaily.org -

Emerging Artist 2013: Kenyon Hansen – Hancock, Michigan

Hansen’s work has a great sense of being sturdy and full of purpose. The surfaces of the pots evoke wear patterns, which are not typical of a material as durable as ceramics, but they refer to age, repetitive use, and therefore personality.

 

Right: Orange box, 8 in. (20 cm) in height, porcelain with sand, soda fired to cone 10, 2012.

 

Below: Handled bowls, 8 in. (20 cm) in length, porcelain with sand, soda fired to cone 10, 2012.

 

 

Vote for your favorite Emerging Artist here!