neilestrick's Profile
Reputation: 38
Excellent
- Group:
- Members
- Active Posts:
- 1,237(1.98 per day)
- Most Active In:
- In the Studio (733 posts)
- Joined:
- 04-October 11
- Profile Views:
- 182,035
- Last Active:
Yesterday, 05:02 PM- Currently:
- Offline
Latest Visitors
-
Pugaboo 
11 Jun 2013 - 17:51 -
MichaelP 
11 Jun 2013 - 08:43 -
GEP 
10 Jun 2013 - 21:53 -
bopper1 
06 Jun 2013 - 15:02 -
Clay Tile Mom 
01 Jun 2013 - 21:27 -
macdoodle 
31 May 2013 - 22:30 -
MerryKate43 
31 May 2013 - 02:08 -
justanassembler 
21 May 2013 - 20:27 -
Min 
21 May 2013 - 04:35 -
mjmiller 
15 May 2013 - 11:57
Posts I've Made
-
In Topic: Schools out, kids at home-In the Studio?
Posted 18 Jun 2013
Have them wedge for the first 12 years, then send them off to college.
-
In Topic: New moderator
Posted 14 Jun 2013
Isn't there some sort of hazing ritual that new moderators have to go through? -
In Topic: Troubleshooting a broken electric potter's wheel
Posted 13 Jun 2013
My bad. I misread and thought it was a Brent. Carry on... -
In Topic: Trials & tribulations with a Skutt 1027
Posted 13 Jun 2013
After 7 years you probably would have seen some corrosion without the cat, but urine would definitely speed it up! I once repaired a kiln that the cat had peed inside of, and when I started it up it I was faced with cat urine steam, which burned into my nostrils and didn't go away for a week.
As for the #8 button turning on the lights on the control board, it actually only shows which relay(s) the control board is currently sending power to. On a single zone kiln it sends power to all 3 at the same time, so all 3 lights should be on at the same time. If not you have a problem with the controller. On multi zone kilns it send power to the relays independently of each other. The controller doesn't know if the relay is actually working or not, just that it's sending power to it. This is a slightly helpful diagnostic tool in multi zone kilns because it will show if a relay is being powered up more often than the others, which could mean there is a problem getting heat to that section due to a bad element or a thermocouple problem, etc. Plus it's fun to watch the lights go on and off. -
In Topic: Troubleshooting a broken electric potter's wheel
Posted 13 Jun 2013
Which model Brent? What does the control box look like. If it's the kind that has the smooth panel and switch, you'll have to replace the whole box. Those were lemons and can't be repaired. If it's another kind, then you've got something in there drawing too much power. Could be the pedal, could be the controller. Brent's are notoriously difficult to diagnose. Whenever I get into them, unless it's something terribly obvious like a fried pedal rheostat, Brent tells me to send in both the pedal and control box. They can't/won't even diagnose them over the phone.
My Information
- Member Title:
- Neil Estrick
- Age:
- Age Unknown
- Birthday:
- Birthday Unknown
- Gender:
-
- Location:
- Grayslake, IL
Contact Information
- E-mail:
- Click here to e-mail me
- Website URL:
-
http://www.neilestrickgallery.com

Sign In
Register
Help

Find Topics
Find Posts
Display name history
Comments
Mary T
23 Feb 2013 - 14:16Mary T
23 Feb 2013 - 13:26Claypple
15 Dec 2012 - 00:36maybe you could give me an advice which kilns are the most reliable? I am interested in firing up to coin 6, middle size,
electric, any voltage.
Thank you in advance.
TJR
30 Nov 2012 - 10:41TJR
22 Aug 2012 - 16:57Tom.
TJR
25 Jul 2012 - 19:13