In Topic: Glaze problem pinholes or blisters
Posted 15 Nov 2012
OffCenter, on 11 November 2012 - 09:50 AM, said:I've been testing a dug clay that is really nice except that every glaze I've tried on it pinholes even with soaks and slow cool downs. I had to bisque up to cone 02 and do a soak to get it to stop pinholeing.
Jim
I think I should bisque fire to the suggestion of cone 04 at least. -
In Topic: Glaze problem pinholes or blisters
Posted 15 Nov 2012
Slurrious, on 10 November 2012 - 11:50 PM, said:blisters/pinholes are sometimes difficult to diagnose/remedy.
there are numerous causes. hopefully, in your case, it's an isolated incident with a glaze you have been using without issue. *if it's a new glaze and not the result of things like dust on bisque ware you need to re-evaluate every ingredient. there are some usual suspects and searches on the digitalfire website will identify most of the culprits.*
we fire to a 04 bisque which helps to alleviate some issues but in the end we've had to abandon a few glazes because of blistering/pinhole issues.
it's fun trying to figure a glaze out but after you've exhausted every internet resource and you are tired of making excuses for that one blister that always shows up - it's time to let the glaze go. for a couple of firings anyway.
re-firing, in my experience, does not work. every glaze has it own personality so hopefully you have some success. we've only ever tried re-firing to the same temperature as the initial firing but we were only trying to fix the most severe cases.
long story short - don't get too attached to a dysfunctional glaze unless you really enjoy testing glazes.
p.s
i learned the hard way that a failing thermocouple will lead to over-firing will lead to blistering so careful your temperature isn't creeping up on you.
*p.p.s.
i really dislike blisters.
**please excuse my failure at reading comprehension. i'm guilty of not reading and understanding the entire thread before braving a reply. it was late - i was tired.
some glazes just refuse to get along.
/lurk
Interesting info and I could be having an issue with a thermocouple. T -
In Topic: Glaze problem pinholes or blisters
Posted 15 Nov 2012
Slurrious, on 10 November 2012 - 11:50 PM, said:blisters/pinholes are sometimes difficult to diagnose/remedy.
there are numerous causes. hopefully, in your case, it's an isolated incident with a glaze you have been using without issue. *if it's a new glaze and not the result of things like dust on bisque ware you need to re-evaluate every ingredient. there are some usual suspects and searches on the digitalfire website will identify most of the culprits.*
we fire to a 04 bisque which helps to alleviate some issues but in the end we've had to abandon a few glazes because of blistering/pinhole issues.
it's fun trying to figure a glaze out but after you've exhausted every internet resource and you are tired of making excuses for that one blister that always shows up - it's time to let the glaze go. for a couple of firings anyway.
re-firing, in my experience, does not work. every glaze has it own personality so hopefully you have some success. we've only ever tried re-firing to the same temperature as the initial firing but we were only trying to fix the most severe cases.
long story short - don't get too attached to a dysfunctional glaze unless you really enjoy testing glazes.
p.s
i learned the hard way that a failing thermocouple will lead to over-firing will lead to blistering so careful your temperature isn't creeping up on you.
*p.p.s.
i really dislike blisters.
**please excuse my failure at reading comprehension. i'm guilty of not reading and understanding the entire thread before braving a reply. it was late - i was tired.
some glazes just refuse to get along.
/lurk -
In Topic: Glaze problem pinholes or blisters
Posted 10 Nov 2012
cambriapottery, on 10 November 2012 - 08:16 PM, said:
neilestrick, on 10 November 2012 - 12:26 PM, said:In general, I would bisque everything to 04. Pinholes typically need a soak or higher firing. Blisters typically need a lower firing or the glaze needs to be stabilized with more clay and/or silica.
How can I identify pinholes or blisters don't they somewhat appear the same? I really appreciate the information on the method used to resolve the two different situations.
If I assume they are pinholes would you refire at a lower cone with a soak? And would it be a cone lower if I go that route and how long a soak would you try? They are glazes made from scratch. -
In Topic: Glaze problem pinholes or blisters
Posted 10 Nov 2012
neilestrick, on 10 November 2012 - 12:26 PM, said:In general, I would bisque everything to 04. Pinholes typically need a soak or higher firing. Blisters typically need a lower firing or the glaze needs to be stabilized with more clay and/or silica.
How can I identify pinholes or blisters don't they somewhat appear the same? I really appreciate the information on the method used to resolve the two different situations.
My Information
- Member Title:
- Member
- Age:
- Age Unknown
- Birthday:
- Birthday Unknown
- Gender:
-
- Location:
- Canada
- Interests:
- gardens, lakes and valleys, forest, streams and rivers, clouds, storms and evening sunsets, birds, bees and flowers
Contact Information
- E-mail:
- Click here to e-mail me
- Website URL:
-
http://cambriapoterie.com/

Sign In
Register
Help

Find Topics
Find Posts
Display name history

Comments
cambriapottery has no profile comments yet. Why not say hello?