  1. Talc bodies

    Posted 2 Apr 2013

    Hi everybody
    I make my own bodies for my ceramic works. The formula is very simple such feldspar, local clay, and china clay (high fired body). Actually the formula has already make me satisfied. But I have read that the body formula can be added talc to lower the vitrified body. Also talc can make the body has a good thermal shocking. I just wanna make sure of that statement. How about whiting? what is the used if added to the body. I really appreciate for any reply.
    Thank you :rolleyes:src="http://ceramicartsdaily.org/community/public/style_emoticons/default/rolleyes.gif">
  2. raw glazing

    Posted 7 Sep 2012

    Hi everyone
    Is this topic has been discussed before? I want to try single firing, so glazing bone dry state. Are there special treatment for this, either the techniques or the materials? because you know, bone dry pot is very frangible in application of the glazes, especially in pouring and dipping techniques. I read the article that we can add flocculant agent like magnesium sulfate and calcium chloride or may be there is another ingredient. Is that true?
    Thank you for your attention.
  3. Again Terra Sig

    Posted 30 Jul 2012

    Hi guys
    About 6 months, my bowl with sig has been displaying in my workshop. But there is oddities when saw the surface body. At the first time, the surface was red shine. But now the surface change into dull red and has black spots. Why this happens?
    I attach the following bowl. Before (mangkok sig) and after (picture 199). I really appreciate for all comments.
  4. Toxic glazes

    Posted 19 Jul 2012

    Hi everyone
    As long as i know, the high fired glazes are safely used for food and beverage containers. But i read in some ceramic books, the glaze that contains barium oxide is harmful even have high fired. Also the glazes that contain chrome, zinc, and cooper. Is that true?
    Is there any technique to determine that the containers are save as containers. I just to make sure that the plate, mug, cup that i have bought safely.
    How about low fired glazes? I think the low fired glazes mostly dangerous as food and beverage containers. How about raku? i see raku wares used as container in Japan. Is that true?Posted Image
  5. Blebbing and blistering

    Posted 2 Jul 2012

    Hi everybody
    I had glaze failures in my works. I used commercial base glaze for my recipes. When I added coloring oxide such mangan, zircon and stain of blue and brown, the glaze had succeed. But added red stain the glaze became blebbing (small air bubbles) and willl be blistering if broken out. Any idea why this happens? Any comment I really appreciate it.

My Information

Member Title:
Advanced Member
Age:
39 years old
Birthday:
August 6, 1973
Gender:
Location:
Bandung, Indonesia
Interests:
I really like slip casting technique. I think anything can be made by molding.

Contact Information

E-mail:
Click here to e-mail me
Website URL:
Website URL  http://www.butterflyceramic.blogspot.com

Comments

Natas Setiabudhi has no profile comments yet. Why not say hello?