Topics I've Started

  1. cone 6 porcelain issues

    Posted 9 Apr 2013

    I am having problems off and on with a fine textural bubbling just under the surface of fired pieces. Using a Grolleg cone 4-6 porcelain fired with the schedule from Mastering Cone 6 Glazes. Ideas????
  2. grolleg porcelain problem

    Posted 9 Jan 2013

    I am a potter of some years and have been working with a Grolleg cone 6 body for the last year or so. I am continually frustrated by bloating. The bisque has been totally fine tuned. The problem is with larger pieces - thrown from 8 to 14 lbs. Is this air trapped in the walls? out gasing? I am firing the schedule from the Cone 6 Glaze guys . . . I am making extra everything for orders to cover the losses. HELP!!

My Information

Member Title:
Newbie
Age:
Age Unknown
Birthday:
Birthday Unknown
Gender:

Contact Information

E-mail:
Private

Friends

pam sinclair hasn't added any friends yet.

Comments

pam sinclair has no profile comments yet. Why not say hello?