Idahopotter's Profile
Reputation: 0
Neutral
- Group:
- Members
- Active Posts:
- 8(0.05 per day)
- Most Active In:
- In the Studio (8 posts)
- Joined:
- 10-December 12
- Profile Views:
- 1,784
- Last Active:
May 23 2013 04:12 PM- Currently:
- Offline
Latest Visitors
-
Idaho Potter 
08 Apr 2013 - 15:34 -
Diane Puckett 
09 Feb 2013 - 12:05 -
R Fraser 
05 Feb 2013 - 17:21 -
Mark C. 
05 Feb 2013 - 02:26 -
Alice Sun 
12 Dec 2012 - 01:05 -
Bobg 
11 Dec 2012 - 13:16 -
pattispots 
10 Dec 2012 - 16:27
Topics I've Started
-
Good Cone 6 Ash Glaze
Posted 9 Feb 2013
Im looking for a good wood ash glaze to fire in a salt kiln. -
Raku firing process
Posted 5 Feb 2013
How long should it take me to fire a trash can raku kiln with a weed burner. -
Make your own bats
Posted 15 Jan 2013
I usually just lift my pots from the wheel head so bats are not something that get used a lot in my studio. My grandfather uses plaster bats which i despise. Any ideas on materials i could make my own bats out of that would be cheaper than buying them. -
What is the best way to cut a chimney
Posted 11 Dec 2012
So I have an electric kiln that i am converting to gas and I need to cut a chimney in the top. The top is a harder metal not your typical electric kiln soft metal. How should I go about cutting it -
?My gas kiln is smoking?
Posted 10 Dec 2012
Ive fired electric for 4 years now. I just got a really old electric kiln for free from the local high school. The kiln is small so I cut only one burner port. I cut out a 7 by 2in chimney. When I began the first test firing it began to smoke within the first 5 min. Not sure why need some advice.
Thanks from Idaho
My Information
- Member Title:
- Member
- Age:
- 19 years old
- Birthday:
- February 10, 1994
- Gender:
-
Contact Information
- E-mail:
- Click here to e-mail me

Sign In
Register
Help

Find Topics
Find Posts
Display name history
Comments
Idaho Potter
08 Apr 2013 - 15:35Idaho Potter
18 Jan 2013 - 17:25