Glaze wrapped. please help!
Posted 21 Oct 2012
Hi,
Used a new glaze for English-cake pans and the glaze (beautiful color - Amaco PC 20 blue rutile) came out of the kiln (cone 5 fire) like it wrapped
The glaze was pretty thick.
Could it be a result of different shrinkage level than the body's?
Thanks
My Information
- Member Title:
- Newbie
- Age:
- Age Unknown
- Birthday:
- Birthday Unknown
- Gender:
-
- Location:
- Galilee, Israel
Contact Information
- E-mail:
- Private
Friends
Galilica hasn't added any friends yet.

Sign In
Register
Help

Find Topics
Find Posts
Display name history
Comments
Galilica has no profile comments yet. Why not say hello?