Topics I've Started
-
Controlling Shrinkage in Casting Slip
Posted 22 Apr 2013
Any advice on how to control the expansion in this low fire white casting slip?
It is shivering off commercial glazes:
.400 TEXAS TALC
.250 C&C
.200 HYDRITE FLAT
.100 MINSPAR 200
.050 VICRON 25-11Any ideas much appreciated !
-
Fireshade Stains /Underglazes
Posted 22 Apr 2013
Anyone have experience with Fireshade underglazes? -
Hold Limitations on Electric Kiln ?
Posted 17 Apr 2013
Question probably for Neil.
Someone was told by one of the kiln companies not to do a hold for more than 30 minutes at high temperature... that it would destroy elements or some such thing.
Sounds like misinformation to me. I could imagine a long hold being extra work for the relays but does anyone know what the kiln maker might have been talking about?
Thanks!
Tim -
Shiho Kanzaki Making Coiled Tea Bowl
Posted 18 Mar 2013
This is great:
Master potter Shiho Kanzaki making a coil/ pinch and throw tea bowl. What a great lesson this is !
http://youtu.be/8T4bsH8XQv4
I tried to mimic what he does exactly: funny but somehow mine did not quite come out the same (;
Anyone have one of these massive banding wheels packed away that you might be willing to part with? Want, want want !
<iframe width="560" height="315" src="http://www.youtube.com/embed/8T4bsH8XQv4" frameborder="0" allowfullscreen></iframe> -
Kintsukuroi Fix
Posted 13 Feb 2013
Hi,
I have a one of a kind cup with a small hole in the side wall.
It's a kooky artsy yunomi type thing so can't really remake it, I know I should smash it but I love it.
I want to try the trick of filling with gold which I think is called Kintsukuroi.
Does anyone know how to do this?
Can i crumple up gold leaf and pack it in there?
Hoping Baymore San or one of you other masters out there might know.
I could fill with epoxy I guess but I doesn't seem right somehow.
Again, I know I should let go and smash it but I really would like to save it if possible.
Thanks!
Tim
My Information
- Member Title:
- Advanced Member
- Age:
- Age Unknown
- Birthday:
- Birthday Unknown
- Gender:
-
- Location:
- MA / NY
- Interests:
-
Wood Firing
Kiln Building
Photography
Contact Information
- E-mail:
- Click here to e-mail me

Sign In
Register
Help

Find Topics
Find Posts
Display name history

Comments
timbo_heff has no profile comments yet. Why not say hello?