Hi everyone. I'm currently working on some arts and crafts forms and looking for a Grueby green / Cucumber green formula that is suited for ^6 oxidation. I would appreciated any suggestions at all. I can't seem to find a clue to this formula on the internet. Anyone out there have experience in this area?? My thanks for any help that can be offered.
Page 1 of 1
Looking For A Grueby Green / Cucumber Formula
#2
Posted 16 January 2011 - 02:25 PM
I have posted a nice matt green from Michael Baileys book ^6 glazes. The recipe is the "comment" under the plate. There are hints of blue and blue dots which were made from a clear glaze over the green.
http://ceramicartsda...ewimage&img=778
Marcia
http://ceramicartsda...ewimage&img=778