hi dears
I want to have glaze recipes in 900'C temprature whithaout stain and whit colorant oxides
does any one can help me?
thank you
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,435
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 16 January 2011 - 09:09 AM

Dear Naghmeh,
900 C is cone 010. That is an unusual temperature for glaze firings. After a fast google for glazes , so far I have not found anything below ^08. I know they exist. Try googling. I searched my library and so far, I have not found any clazes for the temperature. Sorry I can't help.
Good luck.
Marcia
Marcia Selsor
0

#3 User is offline   Rob Hendriks Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 19
  • Joined: 23-October 10
  • LocationThe Netherlands

Posted 16 January 2011 - 10:09 AM

I think you need a high amount of a glazefrit with a low melting point, in your glaze recipe.Some lead and glas frits have low melting points.
0

#4 User is offline   naghmeh Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 23
  • Joined: 04-April 10

Posted 17 January 2011 - 09:04 AM

View PostMarcia Selsor, on 16 January 2011 - 05:39 PM, said:

Dear Naghmeh,
900 C is cone 010. That is an unusual temperature for glaze firings. After a fast google for glazes , so far I have not found anything below ^08. I know they exist. Try googling. I searched my library and so far, I have not found any clazes for the temperature. Sorry I can't help.
Good luck.
Marcia



thank you for your reply
0

#5 User is offline   naghmeh Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 23
  • Joined: 04-April 10

Posted 17 January 2011 - 09:06 AM

View PostRob Hendriks, on 16 January 2011 - 06:39 PM, said:

I think you need a high amount of a glazefrit with a low melting point, in your glaze recipe.Some lead and glas frits have low melting points.



thank you to guide me
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users