Firing Earthenware Glaze With Stoneware Greenware?

#1 User is offline   clayshapes Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 135
  • Joined: 08-January 11
  • LocationToronto

Posted 08 January 2011 - 12:22 PM

I work in both earthenware and stoneware, and fire them separately. But am wondering... Since I bisque my stoneware to 05 and I fire my glazed earthenware to 05 as well (as recommended for the glaze I'm using at the moment), is there a reason why I can't fire them together. I read somewhere that glazed ware in the kiln changes the chemistry somehow and it's not a good idea to mix glazed with unglazed greenware. Any comments on that?
And as a secondary question -- any reason why I can't put stoneware and earthenware into the kiln together for a bisque fire -- since I bisque them at the same cone?
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,435
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 08 January 2011 - 09:17 PM

You should test and see. Some glazes will react to a dirty burnoff from a stoneware bisque in the same chamber. SOme may not react. You can only try it and see what happens in your particular case.
Marcia
Marcia Selsor
0

#3 User is offline   clayshapes Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 135
  • Joined: 08-January 11
  • LocationToronto

Posted 11 January 2011 - 07:19 AM

Thanks. Will give it a try and cross my fingers!