#1 User is offline   clay from the cellar Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 27-November 10
  • LocationMichigan

Posted 27 November 2010 - 10:05 AM

Hello - I have been looking for a mid range olive green glossy glaze for a long time with no success. I decorate many of my pots with a woodland and wildflower theme and would like to add this color to my glaze inventory. Is there anyone that would share a recipe or trade? Thanks so much.
0

#2 User is offline   lakesidepottery Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 18
  • Joined: 16-April 10
  • LocationLakeside Pottery Ceramic School and Studio, Stamford, CT

Posted 29 December 2010 - 02:03 PM

We use a great olive green glaze at our studio and you are wellcome to use the recipe listed on our cone 6 glaze recipes. See some picture below. More pottery tips from Lakeside Pottery

Posted Image



Same glaze applied thicker:

Posted Image

Lakeside Pottery, Ceramic School & Studio
543 Newfield Avenue
Stamford, CT 06905
203-323-2222
www.lakesidepottery.com


Lakeside Pottery, Ceramic School & Studio
543 Newfield Avenue
Stamford, CT 06905
203-323-2222
www.lakesidepottery.com

Posted Image



0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users