Posted 27 September 2010 - 10:25 AM

I have recently purchased a new electric kiln - 100l top loader - it has a pre programmed bisque firing program. My clay is stoneware, and has the following description - 1220°C-1280°C
This jewelof a clay will bring new value to your creations. A smooth white stoneware,with the addition of fine molochite makes an excellent throwing clay suitablefor both oxidising and reduction firing. 10% molochite. As I am self taught I am not sure how long i need to bisque fire for - is it rule of thumb to increase temperature of 100 degrees per hour, up to five hours, then to increase after that, so my firing should be 8 hours ?


The description of the pre programmed bisque firing program in my user manual states the following :


T1 650
Time 1 6:00
T2 900
Time 2 0:00
Tume 3 0:20
Time 4 0


This makes no sense to me though ? Posted ImagePosted ImageAny tips at all would be really welcome as the books that I have do not go into any detail as to how long I need to fire, and to what temperature..



Thanks in advancePosted ImagePosted Image


0

#2 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,370
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 27 September 2010 - 04:38 PM

The pre programmed cycle will do an excellent job for you.
Using it every time will make your firings consistent and your results predictable.

What you need to decide is what cone you want to bisque to ...
Your clay probably has a recommended temp. so use that as a starting point.
Commonly used bisque temps are cone 08, 06 or 04.

I usually use a medium speed but some people prefer the slow.
Better to forget the fast cycle for bisque ware ... You need to take the time to
get rid of the impurities in your clay body.

Hope this helps.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#3 User is offline   Whispering Grass Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 11
  • Joined: 27-September 10
  • LocationIreland

Posted 28 September 2010 - 05:21 AM

Chris,

many thanks for this. The temp quoted on my clay is 1220°C-1280°C
 - not sure what cone this should be fired to - is there a chart I need to refer to re cones temperatures ?


Lorraine


0

#4 User is offline   Deb Evans Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 98
  • Joined: 10-September 10
  • LocationBlue Mtn Lake, NY

Posted 28 September 2010 - 09:32 AM

FYI
your clay temp converts to ^5-9 so its midrange - high fire. I converted celcius to F .
here's temp/cone chart in F degrees = http://www.bigcerami.../ConeChart.html
shows you how to set up cones to double ck/ see how even your high firings are.
0

#5 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,370
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 28 September 2010 - 09:49 AM

Check in the manual that came with your kiln.
Most of them have cone /temp conversion charts in both C and F.
They might also have some suggestions for loading and firing that might be handy.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users