Hi all
last night was my first ever glaze firing, and I came in a little under temp.
Tonight I'm going to give it another shot and I have a couple of questions.

How fast can I ramp up the temperature? do I just start it on high, or go through medium and low first?
I'm going to switch out the witness cone for a new one, should I also change out the kiln-sitter cone?

Since this was my first glaze firing, I had a LOT of glaze tests in there. do you think that re-firing is going to give me a good idea of what the glazes will look like in the future, or should I assume that the tests won't be a good representation?

some technical details: I'm using commercial clay and glazes, using an electric Cress 23 kiln (small studio size). I bisqued to 04, and I was trying to fire to cone 6. my witness cone began to bend, but is still mostly straight, so I estimate that it got to cone 5.

last night's firing was 2 hours on low, 2.5 on medium, and it took 5 hours on HIGH to get to cone 5 (total firing was 10 hours). That seems long to me, I would have expected it to reach temperature a bit faster. does that sound normal to you?
thanks for all your help, this is pretty exciting!!
0

#2 User is offline   gypsy Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 89
  • Joined: 11-April 13
  • LocationJames Creek, Pa

Posted 20 April 2013 - 06:14 PM

View PostJime, on 20 April 2013 - 06:40 PM, said:

Hi all
last night was my first ever glaze firing, and I came in a little under temp.
Tonight I'm going to give it another shot and I have a couple of questions.

How fast can I ramp up the temperature? do I just start it on high, or go through medium and low first?
I'm going to switch out the witness cone for a new one, should I also change out the kiln-sitter cone?

Since this was my first glaze firing, I had a LOT of glaze tests in there. do you think that re-firing is going to give me a good idea of what the glazes will look like in the future, or should I assume that the tests won't be a good representation?

some technical details: I'm using commercial clay and glazes, using an electric Cress 23 kiln (small studio size). I bisqued to 04, and I was trying to fire to cone 6. my witness cone began to bend, but is still mostly straight, so I estimate that it got to cone 5.

last night's firing was 2 hours on low, 2.5 on medium, and it took 5 hours to get to cone 5. That seems long to me, I would have expected it to reach temperature a bit faster. does that sound normal to you?






thanks for all your help, this is pretty exciting!!


It is exciting isn't it? I used to candle then go to medium then high. Now I candle and go straight to high...it works for me.. Good luck on your refire.


0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,400
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 20 April 2013 - 10:22 PM

You are correct. Your results will not be 100% representative of what a single firing would be ... but they might be close enough / might not.

My Cone 5-6 firings take about 6 - 8 hours so that seems OK. Good Luck!
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,509
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 20 April 2013 - 10:53 PM

my ^6 firing are like Chris's... 6 to 8 hours. If your are refining porcelain I would not start on high. 'D be worried about shocking the dense body.
marcia
Marcia Selsor
0

#5 User is offline   Jime Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 02-October 12

Posted 20 April 2013 - 11:12 PM

thanks for the help!
I've got it up and running. New cone and bar, and crossing my fingers for great success. I set it for a "fast firing", and I'm keeping notes on how the dial is moving. It did about 1 hour on low, and 1 hour on medium, just now getting to high... hope it's not too fast!
0

#6 User is offline   High Bridge Pottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 47
  • Joined: 19-February 13
  • LocationNewcastle Upon Tyne

Posted 21 April 2013 - 06:58 AM

I do not know much about firing as I have only done it 10ish times. My firing schedule that got the best results was, 1 hour to 300 centigrade then full whack all the way to 1240 centigrade with a 20 min hold. I have no idea if this is the best but it has given me the best results. Maybe I should take it slower to start. Not sure on the time that it takes from 300 to 1240 but probably 4-6 hours.

Stoneware 'buff', electric kiln, digital controller, too much enthusiasm Posted Image
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users