Doing some experimentation.
I'm using some Laguna Clay WC-520 #16 Transparent
(all-purpose clear gloss glaze which fires from Cone 5 to 10.)as a base over several ^5 bodies including Santa Fe, RSMC,WC-401 B-Mix, and ^10 Soldate.
I've done one firing and found some inconsistency with the oxides vitrifying with the clear, mostly due to imconsistent mixers and brushing and colder spots in the kiln.
I'm doing some upgrades to the to my gas kiln now (bagwall, insulation, etc).
I want to just use red iron oxide, cobalt oxide, and rutile and fire at least to ^5 with a reduction to get everything matured.
What's the water to oxide recipe? What consistency am I looking for for brushing?