Hi,

does anyone know if it is ok to put a transparent food safe glaze over unsafe coloured slips to make bowls food safe? thanks
0

#2 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 965
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 18 March 2013 - 10:22 AM

View Posteoteceramics, on 18 March 2013 - 07:28 AM, said:

Hi,

does anyone know if it is ok to put a transparent food safe glaze over unsafe coloured slips to make bowls food safe? thanks


It's okay and it may work, but it may not. It depends on how "unsafe" the slips are and how well the clear glaze seals them. Testing is the only way to know for sure.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#3 User is offline   eoteceramics Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 48
  • Joined: 17-June 12

Posted 18 March 2013 - 11:38 AM

Thanks Jim, I am confident it will work ok but just don't want to poison anyone !