Wanted to share this tile technique... quick way of making tiny tiles Rate Topic: -----

#1 User is offline   Paula Patton Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 9
  • Joined: 01-August 11
  • LocationBloomington, IN

Posted 15 March 2013 - 01:18 PM

I found a broken light diffuser (grid) at our recycling center and tried a project I had read about before. I couldn't find the article, so I winged it and it worked out! I rolled a slab of clay out, pressed the grid into the clay all the way down and let it dry that way. The next day, tiny tiles fell right out of the grid!! It was like magic! No cutting, no marring, no sanding! They were all perfectly cut to the same size. I glazed them and can now make a great mosaic trivet or, if I make more, something bigger! There are other sizes of light diffusers, I just haven't found one yet!

Attached File(s)


2

#2 User is offline   MadMudder Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 50
  • Joined: 31-March 10
  • LocationMooreville, NC

Posted 15 March 2013 - 01:32 PM

View PostPaula Patton, on 15 March 2013 - 10:18 AM, said:

I found a broken light diffuser (grid) at our recycling center and tried a project I had read about before. I couldn't find the article, so I winged it and it worked out! I rolled a slab of clay out, pressed the grid into the clay all the way down and let it dry that way. The next day, tiny tiles fell right out of the grid!! It was like magic! No cutting, no marring, no sanding! They were all perfectly cut to the same size. I glazed them and can now make a great mosaic trivet or, if I make more, something bigger! There are other sizes of light diffusers, I just haven't found one yet!


OMG what a great tip!! They are so cute, I can see putting them between bigger tiles, framing, color bands, all sorts of stuff.

Thank you! This is exciting...

Beth
MadMudder

Remind me why I'm doing this????
-Beth Ward, Crone Potter
1

#3 User is offline   R Fraser Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 30
  • Joined: 20-October 11
  • LocationThree Lakes, Wisconsin

Posted 15 March 2013 - 01:54 PM

I read a tip somewhere that you can use the same diffuser to mass produce bits of wadding from your favorite wadding formula, just roll it into the diffuser, let it dry a bit and invert. Presto! Never occured to me to make little itty bitty tiles. Could make a very cool mosaic with these!
Richard
So I built a light saber, am I a Jedi now?

0

#4 User is offline   Jess Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 13
  • Joined: 13-June 12
  • LocationVermont

Posted 15 March 2013 - 03:24 PM

View PostPaula Patton, on 15 March 2013 - 01:18 PM, said:

I found a broken light diffuser (grid) at our recycling center and tried a project I had read about before. I couldn't find the article, so I winged it and it worked out! I rolled a slab of clay out, pressed the grid into the clay all the way down and let it dry that way. The next day, tiny tiles fell right out of the grid!! It was like magic! No cutting, no marring, no sanding! They were all perfectly cut to the same size. I glazed them and can now make a great mosaic trivet or, if I make more, something bigger! There are other sizes of light diffusers, I just haven't found one yet!


What a fantastic tip!
0

#5 User is offline   Michaelizabeth Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 05-April 10

Posted 15 March 2013 - 08:19 PM

That is an awesome tip and I can't wait to try it! Thank you for sharing :)
0

#6 User is offline   Roberta12 Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 21
  • Joined: 03-September 12

Posted 15 March 2013 - 09:11 PM

View PostPaula Patton, on 15 March 2013 - 11:18 AM, said:

I found a broken light diffuser (grid) at our recycling center and tried a project I had read about before. I couldn't find the article, so I winged it and it worked out! I rolled a slab of clay out, pressed the grid into the clay all the way down and let it dry that way. The next day, tiny tiles fell right out of the grid!! It was like magic! No cutting, no marring, no sanding! They were all perfectly cut to the same size. I glazed them and can now make a great mosaic trivet or, if I make more, something bigger! There are other sizes of light diffusers, I just haven't found one yet!


I LOVE that idea! I am on the hunt for the light grid!!!! Thanks! I can see many projects ahead with that!



Roberta
0

#7 User is offline   grizzbiz15 Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 22-February 13

Posted 16 March 2013 - 08:51 AM

Great idea!!!
0

#8 User is offline   BeckyH Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 44
  • Joined: 18-April 11

Posted 16 March 2013 - 09:05 PM

To make different size tiles, just cut the grid to the size you want. You can use an exatco knife, or scissors if the grid is thin enough.
1

#9 User is offline   JessicaGrayCeramics Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 11
  • Joined: 06-January 13
  • LocationFeltwell, United Kingdom

Posted 17 March 2013 - 10:50 AM

GREAT IDEA! I love it, thank you for sharing.:)src="http://ceramicartsdaily.org/community/public/style_emoticons/default/smile.gif">
Jessica Gray, MFA
www.JessicaGrayCeramics.com
0

#10 User is online   Mossyrock Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 135
  • Joined: 22-August 10
  • LocationHigh Point, NC

Posted 17 March 2013 - 01:15 PM

This tip opens up a whole other realm of possibilities! I always learn something new from this site.....Love it!
Brenda Moore
Mossy Rock Creations
High Point, NC
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users