Posted 15 March 2013 - 01:26 PM

I moved and my new "studio" is a garage.

I could not throw anymore. I was SOOOOOOO frustrated. Then I noticed (duh) that my garage floor sloped quite a bit. Made it easy to wash out but not very good for other things.

I put a level on my wheel and it was about a 1/4 bubble off the center. I put a nice piece of wood under the 3rd leg of my beloved Brent wheel and suddenly I could throw again. Had to line it up with the slope.

It doesn't take much to throw off throwing : ) but you should check the simple things for a problem. A studio I recently visited had throwing pins for sale. That way when someone wanted throwing pins they were less than a buck and can be put in and easily removed.

Beth
MadMudder

Remind me why I'm doing this????
-Beth Ward, Crone Potter
0

#22 User is offline   Pres Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 994
  • Joined: 02-April 10
  • LocationCentral, PA

Posted 16 March 2013 - 10:16 AM

View PostMadMudder, on 15 March 2013 - 01:26 PM, said:

I moved and my new "studio" is a garage.

I could not throw anymore. I was SOOOOOOO frustrated. Then I noticed (duh) that my garage floor sloped quite a bit. Made it easy to wash out but not very good for other things.

I put a level on my wheel and it was about a 1/4 bubble off the center. I put a nice piece of wood under the 3rd leg of my beloved Brent wheel and suddenly I could throw again. Had to line it up with the slope.

It doesn't take much to throw off throwing : ) but you should check the simple things for a problem. A studio I recently visited had throwing pins for sale. That way when someone wanted throwing pins they were less than a buck and can be put in and easily removed.

Beth


For me, level does matter. If your wheel is out of level 2 degrees on a 9 inch cylinder what is the distance of top variation? Imagine what that is on a 28 or 36 inch cylinder. So I always level my wheel.