Posted 26 February 2013 - 09:21 PM

Hi... I am interested in firing to cone 6 with my Skutt KM 1018. I am playing with stoneware and porcelain. What cone do I use to bisque? Also,which speed do I use for bisque and final firing (slow, med or fast)? I am in no rush... Last question--should I use "ramp/hold"? I've been reading about holding at certain temps for specific amounts of time, but I truly have no idea where to start. I've fired to cone 04 for years and need a change. I would LOVE any help, my greenware is piling up. Thanks in advance!
0

#2 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 110
  • Joined: 13-August 12
  • LocationSW Washington

Posted 27 February 2013 - 11:53 AM

Hi Marge,

I would bisque to cone 04 at a medium rate. I only use the ramp/hold feature when the ware is somewhat think or I suspect it might not be bone dry.
With the ramp hold, I can add a segment for candling to make sure the ware is dry before continuing with the firing.

Use a medium fire rate for the glaze (^6) fire too.

I also use ramp/hold for controlled cooling on glaze fires.

Contact Skutt and they can send you a spreadsheet showing the segments for all the cone to use with the ramp/feature.


Posted Image
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

#3 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,191
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 27 February 2013 - 01:34 PM

Medium speed will work fine for most anything. If you have large or thick pots you may want to bisque on slow.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#4 User is offline   Marge Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 15
  • Joined: 29-January 13

Posted 27 February 2013 - 02:10 PM

Thanks so much!! I can't wait to startPosted Image
0

#5 User is offline   Jo-Ann Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 26
  • Joined: 12-October 11
  • LocationOntario, Canada

Posted 27 February 2013 - 07:48 PM

Hi, I have a skutt but someone a while ago gave me a firing poster for paragon. . . It helped a lot with getting me comfortable with my kiln and giving me a place to start . . . Maybe it can help you . . .

http://www.paragonwe...s/A-82B-FSP.pdf

I have also used this poster

http://www.stonemoun...iring_Chart.pdf
0

#6 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 449
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 28 February 2013 - 09:42 AM

The paragon chart is the same one that was with my paragon kiln that I bought over 40 years ago and still fire, the other chart looks like it would be easy for a novice to use. Denice
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users