: Pyrometer: Skutt 343 vs Fluke 50D? -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Pyrometer: Skutt 343 vs Fluke 50D? Rate Topic: -----

#1 User is offline   TypicalGirl Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 94
  • Joined: 31-March 10
  • LocationAngels Camp, Ca

Posted 26 February 2013 - 08:20 PM

Looking for opinions/input please.

I purchased a spankin' new Skutt model 343 dual input pyrometer last week.
It arrived a few days ago - still in the box, I haven't had a chance to use it yet.
Today, there was a surprise in my mailbox! A friend sent me their old Fluke 50D pyrometer. She says she has only used it once.
It seems the 50D is no longer made, and I'm having a little trouble finding specs on it.

So, I'm wondering if anyone knows the temp range of the Fluke 50d, and if you all have opinions (I expect so) on which pyrometer might be better?
I could potentially return the Skutt and put the money towards [propane or porcelain or, well, you know...
Or if the Skutt might be more accurate or reliable, I can keep the Fluke as a back-up/spare (she only wants a bit of clay in exchange).

Thoughts?
Thanks!
Cathi Newlin, Angels Camp, Ca
box49@caltel.com
http://www.CNewlin.com
0

#2 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,361
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 26 February 2013 - 09:55 PM

Heres the specs for that Fluke
http://www.fluke.com...D.htm?PID=56087

I have 3 flukes and they are all older ones . Fluke is one of the top of the line meter makers. Yours is single input not a dual
so if dual thermocouples in the kiln is what you have you will need the dual input. If not fluke for me is the way to fly-
I do know the Skutts are fairly inexpensive and do not know who the maker is for skutt.
Mark
Mark Cortright
www.liscomhillpottery.com
1

#3 User is offline   TypicalGirl Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 94
  • Joined: 31-March 10
  • LocationAngels Camp, Ca

Posted 26 February 2013 - 10:10 PM

Thanks for the reply Mark!
Actually, this Fluke *is* a dualie! Even came with 2 K-type thermocouples that look as though they've never been used!
Sounds like I really lucked out. Will have to make something really special for my friend.
Cathi Newlin, Angels Camp, Ca
box49@caltel.com
http://www.CNewlin.com
0

#4 User is offline   justanassembler Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 142
  • Joined: 16-May 11
  • LocationBaton Rouge, LA

Posted 27 February 2013 - 07:11 PM

View PostTypicalGirl, on 26 February 2013 - 09:10 PM, said:

Thanks for the reply Mark!
Actually, this Fluke *is* a dualie! Even came with 2 K-type thermocouples that look as though they've never been used!
Sounds like I really lucked out. Will have to make something really special for my friend.


The skutt is actually a TPI instrument--decent meter--Ive used one for a number of woodfirings and been completely satisfied--they seem durable and relatively accurate--as accurate as I'd need in a a pyrometer...
0

#5 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 175
  • Joined: 08-February 12
  • LocationCalifornia

Posted 28 February 2013 - 07:53 PM

i've been using one of those Skutt handheld pyrometers for the past year and a half -- no complaints! bought it to replace a really old Fluke 51 that bit the dust and was going to cost more to repair than buy the Skutt.