Hey World,

I'm mixing up a glaze that uses a yellow stain made with vanaduim so what type of saftey measures should I take when glazing.




Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#2 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 24 February 2013 - 10:47 PM

Check the MSDS sheet from the stain manufacturer. Should list any issues, etc. (Emphasis on "should")
0

#3 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 698
  • Joined: 07-December 11
  • LocationCanada

Posted 25 February 2013 - 09:31 AM

Dust mask. Rubber gloves.