For fun I got a small jar of 2004 high temperature black stain. No where on the jar does it give mixing instructions. I use white stoneware clay and have a lot of dried trimmings but have no clue where to start with stain to dry clay ratio. I sent an email to spectrum last week; no reply yet. I'll experiment but a starting point would be helpful. Thanks :)
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,419
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 25 February 2013 - 12:19 PM

Some underglaze recipes use as much as 25% stain. If the black is strong, start with 10% and add a few grams. Fire the tests and see what increments work best for you.

Marcia
Marcia Selsor
0

#3 User is offline   Jo-Ann Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 26
  • Joined: 12-October 11
  • LocationOntario, Canada

Posted 25 February 2013 - 12:43 PM

Start at 10%. Thank you so much!!!!