I am interested in knowing if anyone has layered glazes using Potter's choice Ironstone. I would like to hear from you especially if you layered it with Ancient Jasper or Deep Firebrick.
0

#2 User is offline   DallasGypsy Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 32
  • Joined: 12-October 11
  • LocationFlorida

Posted 23 February 2013 - 05:50 PM

I've layered it with their Blue Rutile ... looks fabulous!
0

#3 User is offline   Chucwgn Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 14-February 13

Posted 23 February 2013 - 07:09 PM

View PostDallasGypsy, on 23 February 2013 - 05:50 PM, said:

I've layered it with their Blue Rutile ... looks fabulous!


Any pics :-)?
0

#4 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 150
  • Joined: 20-May 12
  • LocationColorado

Posted 23 February 2013 - 07:52 PM

I've painted it under iron lustre.





Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#5 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 150
  • Joined: 20-May 12
  • LocationColorado

Posted 23 February 2013 - 07:58 PM

here is a pic

Attached File(s)


Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users