satin finish satin finish for underglazed sculpture

#1 User is offline   Broken River Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 23-February 13

Posted 23 February 2013 - 01:20 AM

I'd like to give my birds and animals a satin finish. I've tried several commercial earthenware clear satin glazes but they all go milky (Australian - Cesco, Northcote, Walkers). I think it might be better to mix the underglazes with a clear gloss glaze, instead, to give the satin finish. Can anyone advise on proportions and/or glazes? Alternatively, is there a good stoneware, clear satin glaze? I've been using Feeney's Gold Raku and Keanes White Raku Paperclay - both can fire to stoneware.
0

#2 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 134
  • Joined: 20-May 12
  • LocationColorado

Posted 23 February 2013 - 08:02 PM

Cerulean by laguna is a great ^5 green satin glaze.
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#3 User is offline   weeble Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 95
  • Joined: 12-August 12
  • LocationOregon Coast

Posted 24 February 2013 - 12:13 AM

Try just using the underglazes without a top coat. Some of the low-fire underglazes will be satin when overfired to cone 5, but you'll have to do some tests. The colors change a bit at cone 5, but a lot of them work just fine.
Maryjane Carlson

Whistling Fish Pottery
0

#4 User is offline   Broken River Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 23-February 13

Posted 25 February 2013 - 06:05 AM

Many thanks Derek and Maryjane. I'll do some tests.