: Using a mold for a bowl -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Using a mold for a bowl Rate Topic: -----

#1 User is offline   Newbiecw Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 20-January 13

Post icon  Posted 16 February 2013 - 04:23 PM

I am new to pottery and used a metal bowl for a mold. I did spray with WD40, and my instructor told me to take it home and watch it so it didn't dry too long. That was 2 days ago, but I have it wrapped and inside of a covered plastic bin. The clay is still quite wet. I'm really quite unsure how to get it off of the mold. It doesn't seem to want to come off. Did I wait too long or not long enough? How do I know how and when to remove it? (should have asked her for more direction!). Thanks for any help! Cindy
0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,191
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 16 February 2013 - 04:32 PM

Is it on the inside or outside of the bowl?
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#3 User is offline   Newbiecw Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 20-January 13

Posted 16 February 2013 - 07:37 PM

It's on the outside, which I know is trickier because it shrinks.
0

#4 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,356
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 16 February 2013 - 07:52 PM

If its over the outside of the bowl you need to get it off soon. Try some air blown in under rim between clay and metal.
It will crack if it dries onto the form. Try to remove it as soon as it will hold its shape.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#5 User is offline   Claypple Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 121
  • Joined: 15-December 12
  • LocationReno, NV

Posted 22 February 2013 - 08:55 PM

I had a good experience using apples for a mold. Yes, apples!
I needed several medium size round hemispheric forms for one of my projects,
so I cut apples in half and covered them with the rather thin layer of Riverside Grit clay.
It was drying slowly without cracking at all and looked great.
I think any type of vegetables/fruit would work, as long as it is not too perishable.